<?xml version="1.0" encoding="UTF-8"?>
<!DOCTYPE article PUBLIC "-//NLM//DTD JATS (Z39.96) Article Authoring DTD v1.4 20240229//EN" "JATS-articleauthoring1.dtd">
<article article-type="research-article" xml:lang="zh-CN" xmlns:xlink="http://www.w3.org/1999/xlink">
  <front>
    <journal-meta>
      <journal-id journal-id-type="publisher-id">27</journal-id>
      <journal-title-group>
        <journal-title>《机械工程》</journal-title>
        <abbrev-journal-title>Mechanical engineering</abbrev-journal-title>
      </journal-title-group>
      <issn>ISSN：2661-3530(P)/2661-3549(O)</issn>
      <publisher>
        <publisher-name>环宇科学出版社;华文国际出版社</publisher-name>
      </publisher>
    </journal-meta>
    <article-meta>
      <article-id pub-id-type="doi">10.12361/2661-3549-07-05-0381</article-id>
      <article-id pub-id-type="publisher-id">15496</article-id>
      <title-group>
        <article-title>采煤机截齿磨损机理分析</article-title>
      </title-group>
      <contrib-group>
        <contrib contrib-type="author">
          <string-name>魏军强 （陕西陕煤榆北煤业有限公司 陕西榆林 719000）</string-name>
        </contrib>
      </contrib-group>
      <pub-date pub-type="epub">
        <year>2025</year>
        <month>5</month>
      </pub-date>
      <issue>5</issue>
      <abstract>
        <p>在煤炭开采机械化作业中，采煤机截齿作为破碎煤岩的核心部件，其磨损状况直接影响采煤机工作效率与使用寿命，加速磨损不仅降低开 采效率，还会增加维护成本与安全风险。本文围绕采煤机截齿磨损机理展开深入研究，系统分析截齿在井下复杂工况下承受的高频冲击载荷、持续 摩擦作用，以及潮湿环境与腐蚀性介质侵蚀等因素，详细阐述磨料磨损、冲击磨损、腐蚀磨损等主要磨损形式及其产生原因。同时，从截齿材料性 能、采煤机工作参数设置和煤岩固有特性等方面，深入探讨其对截齿磨损进程的影响。旨在为优化截齿设计、改进采煤工艺提供理论依据，通过减 缓截齿磨损速率、延长其服役周期，实现采煤作业经济性与安全性的有效提升。</p>