<?xml version="1.0" encoding="UTF-8"?>
<!DOCTYPE article PUBLIC "-//NLM//DTD JATS (Z39.96) Article Authoring DTD v1.4 20240229//EN" "JATS-articleauthoring1.dtd">
<article article-type="research-article" xml:lang="zh-CN" xmlns:xlink="http://www.w3.org/1999/xlink">
  <front>
    <journal-meta>
      <journal-id journal-id-type="publisher-id">27</journal-id>
      <journal-title-group>
        <journal-title>《机械工程》</journal-title>
        <abbrev-journal-title>Mechanical engineering</abbrev-journal-title>
      </journal-title-group>
      <issn>ISSN：2661-3530(P)/2661-3549(O)</issn>
      <publisher>
        <publisher-name>环宇科学出版社;华文国际出版社</publisher-name>
      </publisher>
    </journal-meta>
    <article-meta>
      <article-id pub-id-type="doi">10.12361/2661-3549-07-05-0397</article-id>
      <article-id pub-id-type="publisher-id">15512</article-id>
      <title-group>
        <article-title>激光雷达饰板于高温下的热变形分析及结构改进</article-title>
      </title-group>
      <contrib-group>
        <contrib contrib-type="author">
          <string-name>张新兵</string-name>
        </contrib>
        <contrib contrib-type="author">
          <string-name>徐作文</string-name>
        </contrib>
        <contrib contrib-type="author">
          <string-name>陈 伟</string-name>
        </contrib>
        <contrib contrib-type="author">
          <string-name>林 鑫 （麦格纳光能汽车饰件系统（杭州）有限公司 浙江杭州 311200）</string-name>
        </contrib>
      </contrib-group>
      <pub-date pub-type="epub">
        <year>2025</year>
        <month>5</month>
      </pub-date>
      <issue>5</issue>
      <abstract>
        <p>针对车顶激光雷达塑料饰板长期暴晒于阳光下导致温度升高发生热变形，从而引发失效问题。本文对塑料饰板尺寸设计并进行热变形仿真， 发现饰板中部底端区域发生形变及应力较大，且存在断裂风险。为通过结构调整来降低应力大小，在饰条初始结构上取消了 C 型槽中加强筋、C 型 槽上部翻边及减小 C 型槽下部翻边宽度并进行相同温度情况下的热变形仿真分析，结果表明，在饰条内外两板中部底端区域变形量显著减小的同时， 其最大应力同样减小。在饰板的生产角度上，本文还提出于饰板中部底端区域增加浇口的措施来减少熔接线的数量，进而减小应力集中。</p>