<?xml version="1.0" encoding="UTF-8"?>
<!DOCTYPE article PUBLIC "-//NLM//DTD JATS (Z39.96) Article Authoring DTD v1.4 20240229//EN" "JATS-articleauthoring1.dtd">
<article article-type="research-article" xml:lang="zh-CN" xmlns:xlink="http://www.w3.org/1999/xlink">
  <front>
    <journal-meta>
      <journal-id journal-id-type="publisher-id">27</journal-id>
      <journal-title-group>
        <journal-title>《机械工程》</journal-title>
        <abbrev-journal-title>Mechanical engineering</abbrev-journal-title>
      </journal-title-group>
      <issn>ISSN：2661-3530(P)/2661-3549(O)</issn>
      <publisher>
        <publisher-name>环宇科学出版社;华文国际出版社</publisher-name>
      </publisher>
    </journal-meta>
    <article-meta>
      <article-id pub-id-type="doi">10.12421/jxgc2661-3549-202510072</article-id>
      <article-id pub-id-type="publisher-id">22303</article-id>
      <title-group>
        <article-title>输送机中部槽激光修复及表面强化技术的研究与应用</article-title>
      </title-group>
      <contrib-group>
        <contrib contrib-type="author">
          <string-name>赵琦 黄陵县店头镇黄陵鑫桥公司</string-name>
        </contrib>
      </contrib-group>
      <pub-date pub-type="epub">
        <year>2025</year>
        <month>10</month>
      </pub-date>
      <issue>10</issue>
      <abstract>
        <p>刮板输送机作为现代化综采工作面的关键运输设备，其核心部件中部槽的耐久性直接影响到整个采煤系统的运行效率与可靠性。中部槽在恶劣工况下长期承受强磨损、高冲击负荷，导致其表面迅速失效。本文系统综述了激光修复与表面强化技术在中部槽维护领域的研究进展与应用实践，重点分析了激光熔覆、激光-MAG复合焊接、激光冲击强化等关键技术原理、材料体系及实施效果。研究表明，激光修复技术可使中部槽寿命延长2-3倍，大幅降低设备维护成本。最后，本文展望了该领域面临的技术挑战与未来发展趋势，为中部槽长效服役提供技术参考。</p>