<?xml version="1.0" encoding="UTF-8"?>
<!DOCTYPE article PUBLIC "-//NLM//DTD JATS (Z39.96) Article Authoring DTD v1.4 20240229//EN" "JATS-articleauthoring1.dtd">
<article article-type="research-article" xml:lang="zh-CN" xmlns:xlink="http://www.w3.org/1999/xlink">
  <front>
    <journal-meta>
      <journal-id journal-id-type="publisher-id">27</journal-id>
      <journal-title-group>
        <journal-title>《机械工程》</journal-title>
        <abbrev-journal-title>Mechanical engineering</abbrev-journal-title>
      </journal-title-group>
      <issn>ISSN：2661-3530(P)/2661-3549(O)</issn>
      <publisher>
        <publisher-name>环宇科学出版社;华文国际出版社</publisher-name>
      </publisher>
    </journal-meta>
    <article-meta>
      <article-id pub-id-type="publisher-id">9565</article-id>
      <title-group>
        <article-title>DR 技术在 PE 管焊口检测上的应用研究</article-title>
      </title-group>
      <contrib-group>
        <contrib contrib-type="author">
          <string-name>贺 睿 1 徐先满 2 王平松 2 （1</string-name>
        </contrib>
        <contrib contrib-type="author">
          <string-name>铜陵市特种设备监督检验中心 安徽铜陵 244000</string-name>
        </contrib>
        <contrib contrib-type="author">
          <string-name>2 安徽华夏高科技开发有限责任公司 安徽合肥 231131）</string-name>
        </contrib>
      </contrib-group>
      <pub-date pub-type="epub">
        <year>2024</year>
        <month>12</month>
      </pub-date>
      <issue>12</issue>
      <abstract>
        <p>PE 管采用热熔或电熔焊接，焊接质量直接影响管道的安全，而将 DR 技术应用于 PE 管检测，能够快
速检测电熔焊中的未融合，电阻丝错位等以及热熔焊中的孔洞等缺陷，通过对消缺，对 PE 管的安全运行有重要
的现实意义。</p>