<?xml version="1.0" encoding="UTF-8"?>
<!DOCTYPE article PUBLIC "-//NLM//DTD JATS (Z39.96) Article Authoring DTD v1.4 20240229//EN" "JATS-articleauthoring1.dtd">
<article article-type="research-article" xml:lang="zh-CN" xmlns:xlink="http://www.w3.org/1999/xlink">
  <front>
    <journal-meta>
      <journal-id journal-id-type="publisher-id">29</journal-id>
      <journal-title-group>
        <journal-title>《建筑施工与发展》</journal-title>
        <abbrev-journal-title>CONSTRUCTION AND DEVEL OPMENT</abbrev-journal-title>
      </journal-title-group>
      <issn>ISSN：2737-4262；EISSN:2705-1269</issn>
      <publisher>
        <publisher-name>华文科学出版社</publisher-name>
      </publisher>
    </journal-meta>
    <article-meta>
      <article-id pub-id-type="doi">10.12361/2705-1269-7310-86</article-id>
      <article-id pub-id-type="publisher-id">17258</article-id>
      <title-group>
        <article-title>污泥淤泥制备轻骨料混凝土低碳方案探析</article-title>
      </title-group>
      <contrib-group>
        <contrib contrib-type="author">
          <string-name>李 赢 冯 磊 杨志鹏 吴昊芮 董珈瑞 冯琬淇 吴欣彤</string-name>
        </contrib>
      </contrib-group>
      <pub-date pub-type="epub">
        <year>2025</year>
        <month>10</month>
      </pub-date>
      <issue>10</issue>
      <abstract>
        <p>在全球碳中和目标驱动下，探索建筑固废资源化利用与低碳建材开发成为行业迫切需求。本研究以污水厂污泥与河道淤泥烧结制
备的轻质陶粒为粗骨料，开展轻骨料混凝土配制技术研究。系统调控水胶比和水泥用量，讨论了其对混凝土工作性、力学性能及热工性能
的影响。确定了最优配比（水胶比 0.45，水泥 250kg/m3
，总胶材 420kg/m3
），所得混凝土性能全面满足 LC15 结构保温轻骨料混凝土标准要
求。证实利用污泥陶粒替代天然骨料制备达标混凝土具有可行性。
关键词：污泥淤泥；轻骨料混凝土；配合比设计；低碳</p>