<?xml version="1.0" encoding="UTF-8"?>
<!DOCTYPE article PUBLIC "-//NLM//DTD JATS (Z39.96) Article Authoring DTD v1.4 20240229//EN" "JATS-articleauthoring1.dtd">
<article article-type="research-article" xml:lang="zh-CN" xmlns:xlink="http://www.w3.org/1999/xlink">
  <front>
    <journal-meta>
      <journal-id journal-id-type="publisher-id">29</journal-id>
      <journal-title-group>
        <journal-title>《建筑施工与发展》</journal-title>
        <abbrev-journal-title>CONSTRUCTION AND DEVEL OPMENT</abbrev-journal-title>
      </journal-title-group>
      <issn>ISSN：2737-4262；EISSN:2705-1269</issn>
      <publisher>
        <publisher-name>华文科学出版社</publisher-name>
      </publisher>
    </journal-meta>
    <article-meta>
      <article-id pub-id-type="doi">10.12421/JZSGYFZ2705-1269-080234</article-id>
      <article-id pub-id-type="publisher-id">26054</article-id>
      <title-group>
        <article-title>生活垃圾焚烧厂冷却塔环境腐蚀分析</article-title>
      </title-group>
      <contrib-group>
        <contrib contrib-type="author">
          <string-name>陈 昆 中城院（北京）环境科技股份有限公司</string-name>
        </contrib>
      </contrib-group>
      <pub-date pub-type="epub">
        <year>2026</year>
        <month>2</month>
      </pub-date>
      <issue>2</issue>
      <abstract>
        <p>为了研究生活垃圾焚烧厂冷却塔在恶劣环境下腐蚀问题，本文以某焚烧发电厂冷却塔为工程案例，通过现场腐蚀调查与检测、水
质和大气环境数据分析，对冷却塔的腐蚀特征及原因进行了系统的研究。结果显示，高浓度氯离子侵蚀、酸性气体化学腐蚀是造成混凝土
中性化、钢筋锈蚀和结构劣化的主要原因。在此基础上提出以材料体系优化、阴极保护设计、运行参数调节为内容的综合治理措施，为焚
烧厂冷却塔耐久性设计和运维管理提供技术上的参考。
关键词：生活垃圾焚烧厂；冷却塔；氯离子侵蚀；混凝土劣化</p>