<?xml version="1.0" encoding="UTF-8"?>
<!DOCTYPE article PUBLIC "-//NLM//DTD JATS (Z39.96) Article Authoring DTD v1.4 20240229//EN" "JATS-articleauthoring1.dtd">
<article article-type="research-article" xml:lang="zh-CN" xmlns:xlink="http://www.w3.org/1999/xlink">
  <front>
    <journal-meta>
      <journal-id journal-id-type="publisher-id">8</journal-id>
      <journal-title-group>
        <journal-title>《科技研究》</journal-title>
      </journal-title-group>
      <issn>ISSN:3079-9244（原2717-5480）</issn>
      <publisher>
        <publisher-name>华文科学出版社</publisher-name>
      </publisher>
    </journal-meta>
    <article-meta>
      <article-id pub-id-type="doi">10.12421/ddyx3079-9244-2025437</article-id>
      <article-id pub-id-type="publisher-id">18496</article-id>
      <title-group>
        <article-title>2A12 铝合金薄板加工去除量及特征对其变形的影响与研究</article-title>
      </title-group>
      <contrib-group>
        <contrib contrib-type="author">
          <string-name>左锋 焦海亮 杨金上 (北方自动控制技术研究所 山西太原 030006)</string-name>
        </contrib>
      </contrib-group>
      <pub-date pub-type="epub">
        <year>2025</year>
        <month>4</month>
      </pub-date>
      <issue>4</issue>
      <abstract>
        <p>本论文研究探讨了加工去除量及特征对 2A12 铝合金薄板零件变形的影响。实验采用经时效处理校平的 2A12-T4
铝合金薄板，利用三坐标测量机对比加工前后平面度变化。仿真与实验结果表明，当去除面积为 30%和加工特征为凹槽加筋
时，零件变形最小。具体而言，去除面积为 30%时，变形量仅为 0.59%；加工特征为凹槽加筋时，变形量为 77.21%。研究表
明，合理选择加工去除量与特征可有效降低薄板零件变形，提升其精度。</p>