<?xml version="1.0" encoding="UTF-8"?>
<!DOCTYPE article PUBLIC "-//NLM//DTD JATS (Z39.96) Article Authoring DTD v1.4 20240229//EN" "JATS-articleauthoring1.dtd">
<article article-type="research-article" xml:lang="zh-CN" xmlns:xlink="http://www.w3.org/1999/xlink">
  <front>
    <journal-meta>
      <journal-id journal-id-type="publisher-id">8</journal-id>
      <journal-title-group>
        <journal-title>《科技研究》</journal-title>
      </journal-title-group>
      <issn>ISSN:3079-9244（原2717-5480）</issn>
      <publisher>
        <publisher-name>华文科学出版社</publisher-name>
      </publisher>
    </journal-meta>
    <article-meta>
      <article-id pub-id-type="doi">10.12421/kjyj3079-9244-2026-4-75</article-id>
      <article-id pub-id-type="publisher-id">27553</article-id>
      <title-group>
        <article-title>汽车关键安全部件用热冲压成形 22MnB5 钢激光焊接工艺研究</article-title>
      </title-group>
      <contrib-group>
        <contrib contrib-type="author">
          <string-name>王绘程 孙岩 刘辉* 刘洋 郎鲲 （长春工程学院 机电工程学院 长春 130012）</string-name>
        </contrib>
      </contrib-group>
      <pub-date pub-type="epub">
        <year>2026</year>
        <month>4</month>
      </pub-date>
      <issue>4</issue>
      <abstract>
        <p>采用 YLS-2000 激光器对汽车关键安全部件用热冲压成形 22MnB5 钢进行激光对焊试验，设计了三因素三水平正交实验并进行结果分析，探究激光焊接工艺参数对焊缝成形、显微组织及力学性能的影响，获得激光对焊条件下最优工艺。结果表明:在激光功率 1000W，焊接速度 15mm/s，离焦量 0 的工艺条件下，获得的焊接接头强度最高。热冲压成形后 22MnB5钢激光对焊焊缝区组织主要为板条马氏体，近缝区为粗大板条状马氏体，靠近母材区为细小板条状马氏体。接头断裂位置位于热影响区，断口特征为韧脆混合断裂。</p>
      </abstract>